Polymer Property : Izod Impact, Notched (ISO) = 8.82 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 8.82 kJ/m²

@Temperature 22.8 °C
4.20 ft-lb/in²

@Temperature 73.0 °F
ISO 180/1A
Polymer Resources PEI-GP1-TFE5 Polyetherimide, 5% PTFE, Flame Retardant
Polyetherimide, General Purpose, 5% PTFE, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
Izod Impact, Notched (ISO) 8.82 kJ/m²

@Temperature 22.8 °C
4.20 ft-lb/in²

@Temperature 73.0 °F
ISO 180/1A
ExxonMobil AP3AW Polypropylene Impact Copolymer
Product Description: A UV stabilized medium impact copolymer resin designed for automotive battery cases.Availability: Asia Pacific Features:Good UV ResistanceHigh StiffnessLow WarpageMedium FlowMe..