Polymer Property : Izod Impact, Notched (ISO) = 7.35 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 7.35 kJ/m²

@Temperature -30.0 °C
3.50 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
Polymer Resources ABS-GP1 General Purpose ABS
General Purpose Acrylonitrile Butadiene StyreneFeatures: • Medium Impact ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig..
Izod Impact, Notched (ISO) 7.35 kJ/m²

@Temperature -30.0 °C
3.50 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
Polymer Resources ABS-GP1-[color]-EP General Purpose ABS, Electroplating Grade
General Purpose Acrylonitrile Butadiene Styrene, Electroplating GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam..
Izod Impact, Notched (ISO) 7.35 kJ/m²

@Temperature -30.0 °C
3.50 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
Polymer Resources ABS-GP1-[color]-UV General Purpose ABS, UV-stabilized
General Purpose Acrylonitrile Butadiene Styrene, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.In..
Izod Impact, Notched (ISO) 7.35 kJ/m²

@Temperature -30.0 °C
3.50 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
Polymer Resources PEI-GP1-TFE5 Polyetherimide, 5% PTFE, Flame Retardant
Polyetherimide, General Purpose, 5% PTFE, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
Izod Impact, Notched (ISO) 7.35 kJ/m²

@Temperature 22.8 °C
3.50 ft-lb/in²

@Temperature 73.0 °F
ISO 180/1A
ExxonMobil PP7555KNE2 Polypropylene Impact Copolymer
Product Description: A high melt flow rate medium impact copolymer resin designed for thin wall injection molding requiring fast cycle time and low odor.Availability: Asia Pacific Features:Good Mol..