Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 6.70 kJ/m² @Temperature -20.0 °C |
3.19 ft-lb/in² @Temperature -4.00 °F |
ISO 180/1eA |
Polyplastic Armlen® PP-10IM-901 Polypropylene, Mineral Filled Information provided by PolyPlastic Group. |