Polymer Property : Izod Impact, Notched (ISO) = 3.19 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 6.70 kJ/m²

@Temperature -20.0 °C
3.19 ft-lb/in²

@Temperature -4.00 °F
ISO 180/1eA
Polyplastic Armlen® PP-10IM-901 Polypropylene, Mineral Filled
Information provided by PolyPlastic Group.