Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 105 kJ/m²

@Temperature 23.0 °C
50.0 ft-lb/in²

@Temperature 73.4 °F
cond.; ISO 180-1A
Lanxess Durethan® BC 550 Z DUSXBL 900116 Nylon 6, Impact Modified
PA 6, non-reinforced, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS.