Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 41.0 kJ/m²

@Temperature 23.0 °C
19.5 ft-lb/in²

@Temperature 73.4 °F
ISO 180
LyondellBasell Hostacomâ„¢ CB275FC Thermoplastic Polyolefin Elastomer
Description: Hostacomâ„¢ CB275FC high melt flow, 1,900 MPa flexural modulus, precolored, UV-stabilized, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent balance of pro..
Izod Impact, Notched (ISO) 41.0 kJ/m²

@Temperature 23.0 °C
19.5 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Cycoloy® C1100 PC+ABS (Europe-Africa-Middle East)
CYCOLOY C1100 is a PC+ABS blend developed to satisfy the demanding application requirements, where optimum combination is needed of superior processing efficiency, excellent ductility also at sub ze..