Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 83.0 kJ/m² @Temperature 23.0 °C |
39.5 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
BASF Ultramid® AZ HP UV BK 23220 PA66 (Dry) Description: Ultramid A3Z HP UV BK23220 is an impact modified PA66 containing heat and ultraviolet light stabilizers. Designed for maximum toughness at low temperatures, Ultramid A3Z HP UV BK23220 o.. |