Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 63.0 kJ/m²

@Temperature -30.0 °C
30.0 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® EXRL0684 PC Copolymer
7 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched (ISO) 63.0 kJ/m²

@Temperature 23.0 °C
30.0 ft-lb/in²

@Temperature 73.4 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® FXD9810U PC Copolymer (Asia Pacific)
Polycarbonate with high flow, excellent processability, good impact and thermal properties, UV stabilized, non-Chlorine and non-Bromine flame retardant, UL rated V-0 and V-1. Available in limited di..
Izod Impact, Notched (ISO) 63.0 kJ/m²

@Temperature 23.0 °C
30.0 ft-lb/in²

@Temperature 73.4 °F
ISO 180-4A
Styron Pulse® 2000EZ PC/ABS
Engineering ResinInformation provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Izod Impact, Notched (ISO) 63.0 kJ/m²

@Temperature 23.0 °C
30.0 ft-lb/in²

@Temperature 73.4 °F
ISO 180/A
Styron PULSEâ„¢ 2000 EZ PC/ABS Engineering Resin
Overview: PULSE 2000 Engineering Resin is designed to provide top performance in tough applications, from single piece items to intricate components. Ideal for energy management solutions, it can wi..