Polymer Property : Izod Impact, Notched (ISO) = 3.00 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 6.30 kJ/m²

@Temperature -30.0 °C
3.00 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
Polymer Resources ABS-FR Flame Retardant ABS
Flame Retardant Acrylonitrile Butadiene StyreneFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch..
Izod Impact, Notched (ISO) 6.30 kJ/m²

@Temperature -30.0 °C
3.00 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
Polymer Resources ABS-FR-[color]-UV Flame Retardant ABS, UV-stabilized
Flame Retardant Acrylonitrile Butadiene Styrene, UV-stabilizedFeatures: • Flame Retardant • Self Extinguishing • Good UV ResistanceProcess: Injection MoldingNotes: All physical, mechanical and..
Izod Impact, Notched (ISO) 6.30 kJ/m²

@Temperature -30.0 °C
3.00 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
Polymer Resources ABS-GP-HH General Purpose ABS, High Heat
General Purpose Acrylonitrile Butadiene Styrene, High HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
Izod Impact, Notched (ISO) 6.30 kJ/m²

@Temperature -40.0 °C
3.00 ft-lb/in²

@Temperature -40.0 °F
ISO 180
Eastman DuraStar DS2000 Polymer, Natural
Durastar DS2000 polymer has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing characteristics. DS2000 has ver..
Izod Impact, Notched (ISO) 6.30 kJ/m²

@Temperature -40.0 °C
3.00 ft-lb/in²

@Temperature -40.0 °F
ISO 180
Eastman DuraStar DS2110UVI Polymer, Natural
Durastar DS2110UVI polymer, contains an ultraviolet light stabilization package. It is recommended for indoor applications requiring enhanced color stability upon extended exposure to fluorescent li..
Izod Impact, Notched (ISO) 6.30 kJ/m²

@Temperature -40.0 °C
3.00 ft-lb/in²

@Temperature -40.0 °F
ISO 180
Eastman DuraStar MN621 Polymer, Natural
Durastar Polymer MN621 was developed for the medical device industry and contains a mold release It processes easily and requires minimal drying time. It has superior toughness, high clarity and goo..
Izod Impact, Notched (ISO) 6.30 kJ/m²

@Temperature -40.0 °C
3.00 ft-lb/in²

@Temperature -40.0 °F
ISO 180
Eastman Eastar BR203 Copolyester
Eastar BR203 Copolyester contains a mold release additive. It has excellent appearance and is nearly water-clear. Its most outstanding features are its chemical resistance and processing capabilitie..