Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 1.28 kJ/m² @Temperature 23.0 °C |
0.609 ft-lb/in² @Temperature 73.4 °F |
ISO 180/4A |
Styron Magnumâ„¢ 375 HP Acrylonitrile Butadiene Styrene (ABS) High Heat, Low Gloss ABS.Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |