Material Notes:
High Heat, Low Gloss ABS.Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Physical Properties Metric English Comments
Density 1.062 g/cc
0.03837 lb/in³
ISO 1183
Melt Flow 2.4 g/10 min

@Load 3.80 kg,
Temperature 230 °C
2.4 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 43.8 MPa
6350 psi
50mm/min; ISO 527
Elongation at Break 5.0 %
5.0 %
50mm/min; ISO 527
Flexural Modulus 2.235 GPa
324.2 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 0.890 kJ/m²

@Temperature -30.0 °C
0.424 ft-lb/in²

@Temperature -22.0 °F
ISO 180/4A
1.28 kJ/m²

@Temperature 23.0 °C
0.609 ft-lb/in²

@Temperature 73.4 °F
ISO 180/4A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
unannealed; ISO 75-A
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °C
183 °F
unannealed; ISO 75-A