Polymer Property : Four Ball Wear = 0.590 mm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Four Ball Wear 0.590 mm
0.0232 in
1 hr. @ 1200 rpm, 75°C (167°F), 40 kg.; ASTM D-2266
ConocoPhillips ANDEROL® 783-1 Series Synthetic Food Grade Greases, NLGI Grade 1
Description: ANDEROL 783 Series Greases are made from synthetic hydrocarbons (PAO) and an aluminum complex soap thickener, allowing for a wide range of operating temperatures. The 783 Series Greases..