Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Four Ball Wear | 0.470 mm | 0.0185 in | |
ELM® SoyGrease™ EP Premium Biodegradable Extreme Pressure Grease, NLGI Grade 2 Description: ELM SoyGrease™ EP Premium grease is a premium quality biodegradable, water resistant, Biotechbased™ grease formulated with OptiBase™ Oils, lithium-based thickener and extreme press.. |
|||
Four Ball Wear | 0.470 mm | 0.0185 in | |
ELM® SoyGrease™ EP Premium Biodegradable Extreme Pressure Grease, NLGI Grade 3 Biodegradable Extreme Pressure GreaseInformation provided by ELM® |