Polymer Property : Four Ball Wear = 0.0185 in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Four Ball Wear 0.470 mm
0.0185 in
ELM® SoyGrease™ EP Premium Biodegradable Extreme Pressure Grease, NLGI Grade 2
Description: ELM SoyGrease™ EP Premium grease is a premium quality biodegradable, water resistant, Biotechbased™ grease formulated with OptiBase™ Oils, lithium-based thickener and extreme press..
Four Ball Wear 0.470 mm
0.0185 in
ELM® SoyGrease™ EP Premium Biodegradable Extreme Pressure Grease, NLGI Grade 3
Biodegradable Extreme Pressure GreaseInformation provided by ELM®