Polymer Property : Four Ball Wear = 0.450 mm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Four Ball Wear 0.450 mm
0.0177 in
Wear Scar
ConocoPhillips Tacna® EP Polyurea Grease NLGI Grade 1
Description: Conoco Tacna EP Polyurea Grease is a shear-stable product with exceptional extreme-pressure characteristics and excellent water resistance. It is recommended for use in steel mills, off..
Four Ball Wear 0.450 mm
0.0177 in
ASTM D942
ConocoPhillips Tacna® HD Grease NLGI Grade 1
Tacna HD is a premium quality, adhesive, extreme-pressure (EP) lithium complex grease developed for the lubrication of heavily loaded construction, mining and industrial equipment. It also is recomm..
Four Ball Wear 0.450 mm
0.0177 in
Scar Wear; ASTM D2266
ConocoPhillips Tacna® HD Grease NLGI Grade 2
Tacna HD is a premium quality, adhesive, extreme-pressure (EP) lithium complex grease developed for the lubrication of heavily loaded construction, mining and industrial equipment. It also is recomm..
Four Ball Wear 0.450 mm
0.0177 in
ChevronTexaco Delo® NLGI 0 Grease EP
FeaturesChevron Delo Greases EP are technically advanced, extreme pressure greases for a wide variety of on- and off-road applications.They are formulated with ISOSYN® base stocks, a lithium comple..
Four Ball Wear 0.450 mm
0.0177 in
ChevronTexaco Delo® NLGI 00 Grease EP
FeaturesChevron Delo Greases EP are technically advanced, extreme pressure greases for a wide variety of on- and off-road applications.They are formulated with ISOSYN® base stocks, a lithium comple..
Four Ball Wear 0.450 mm
0.0177 in
ChevronTexaco Delo® NLGI 1 Grease EP
FeaturesChevron Delo Greases EP are technically advanced, extreme pressure greases for a wide variety of on- and off-road applications.They are formulated with ISOSYN® base stocks, a lithium comple..
Four Ball Wear 0.450 mm
0.0177 in
ChevronTexaco Delo® NLGI 2 Grease EP
FeaturesChevron Delo Greases EP are technically advanced, extreme pressure greases for a wide variety of on- and off-road applications.They are formulated with ISOSYN® base stocks, a lithium comple..
Four Ball Wear 0.450 mm
0.0177 in
ChevronTexaco FM ISO 32 Lubricating Oil
Chevron Lubricating Oils FM are premium performance industrial lubricants designed for use in the food processing and other sensitive industries where incidental food contact may occur. Chevron Lubr..
Four Ball Wear 0.450 mm
0.0177 in
ConocoPhillips 100 Super Hydraulic Oil
Description: Conoco Super Hydraulic Oil is a high-quality antiwear hydraulic fluid formulated from premium Conoco hydrocracked base stocks to provide superior water separation, antiwear protection, ..
Four Ball Wear 0.450 mm
0.0177 in
ConocoPhillips 100 Ultra-Clean Super Hydraulic Oil
Description: Conoco Ultra-Clean Super Hydraulic Oils have the same high performance characteristics of regular Super Hydraulic Oils with the added advantage of a guaranteed ISO cleanliness code of 1..
Four Ball Wear 0.450 mm
0.0177 in
ConocoPhillips 32 Super Hydraulic Oil
Description: Conoco Super Hydraulic Oil is a high-quality antiwear hydraulic fluid formulated from premium Conoco hydrocracked base stocks to provide superior water separation, antiwear protection, ..
Four Ball Wear 0.450 mm
0.0177 in
ConocoPhillips 46 Super Hydraulic Oil
Description: Conoco Super Hydraulic Oil is a high-quality antiwear hydraulic fluid formulated from premium Conoco hydrocracked base stocks to provide superior water separation, antiwear protection, ..
Four Ball Wear 0.450 mm
0.0177 in
1 hr. @ 1200 rpm, 75°C (167°F), 40 kg.; ASTM D-4172
ConocoPhillips ANDEROL® AA Cooker & Valve Oil, High Temperature Water Resistant Food Grade ISO 220
Description: ANDEROL PQ AA Cooker & Valve Oil is a white mineral oil based product that meets the former H-1 approval requirements of the USDA where incidental food contact can occur. PQ AA Cooker &..
Four Ball Wear 0.450 mm
0.0177 in
ConocoPhillips MV22 Super Hydraulic Oil
Description: Conoco Super Hydraulic Oil is a high-quality antiwear hydraulic fluid formulated from premium Conoco hydrocracked base stocks to provide superior water separation, antiwear protection, ..
Four Ball Wear 0.450 mm
0.0177 in
Scar Diameter
ELM® SoyEasy™ OGL Biodegradable – Biobased Open Gear Lubricant
Description: SoyEasy - OGL is a premium quality biodegradable open gear lubricant formulated with the best optimized Biotechbased™ USA-grown natural seed oil that surpasses the lubricity of most c..
Four Ball Wear 0.450 mm
0.0177 in
ConocoPhillips 150 Super Hydraulic Oil
Description: Conoco Super Hydraulic Oil is a high-quality antiwear hydraulic fluid formulated from premium Conoco hydrocracked base stocks to provide superior water separation, antiwear protection, ..
Four Ball Wear 0.450 mm
0.0177 in
ConocoPhillips 46 Ultra-Clean Super Hydraulic Oil
Description: Conoco Ultra-Clean Super Hydraulic Oils have the same high performance characteristics of regular Super Hydraulic Oils with the added advantage of a guaranteed ISO cleanliness code of 1..
Four Ball Wear 0.450 mm
0.0177 in
ConocoPhillips 68 Super Hydraulic Oil
Description: Conoco Super Hydraulic Oil is a high-quality antiwear hydraulic fluid formulated from premium Conoco hydrocracked base stocks to provide superior water separation, antiwear protection, ..
Four Ball Wear 0.450 mm
0.0177 in
ConocoPhillips 68 Ultra-Clean Super Hydraulic Oil
Description: Conoco Ultra-Clean Super Hydraulic Oils have the same high performance characteristics of regular Super Hydraulic Oils with the added advantage of a guaranteed ISO cleanliness code of 1..
Four Ball Wear 0.450 mm
0.0177 in
ConocoPhillips MV32 Super Hydraulic Oil
Description: Conoco Super Hydraulic Oil is a high-quality antiwear hydraulic fluid formulated from premium Conoco hydrocracked base stocks to provide superior water separation, antiwear protection, ..
Four Ball Wear 0.450 mm
0.0177 in
ConocoPhillips 22 Super Hydraulic Oil
Description: Conoco Super Hydraulic Oil is a high-quality antiwear hydraulic fluid formulated from premium Conoco hydrocracked base stocks to provide superior water separation, antiwear protection, ..
Four Ball Wear 0.450 mm
0.0177 in
ConocoPhillips 32 Ultra-Clean Super Hydraulic Oil
Description: Conoco Ultra-Clean Super Hydraulic Oils have the same high performance characteristics of regular Super Hydraulic Oils with the added advantage of a guaranteed ISO cleanliness code of 1..