Polymer Property : Four Ball Extreme Pressure, Weld Load = 50.0 kg Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 50.0 kg
110 lb (mass)
Mean Hertz Load; IP 239
Solvay Specialty Polymers FOMBLIN® LC08 PFPE Lubricant
FOMBLIN LC perfluoropolyether fluids have the following unique features: excellent wear characteristics; very good low temperature properties; cost-effective; and outstanding for applications requir..
Four Ball Extreme Pressure, Weld Load 50.0 kg
110 lb (mass)
Load Weld Index
ChevronTexaco ISO 460 Ultra Gear Lubricant
FeaturesChevron Ultra Gear Lubricants are premium grade, multipurpose gear lubricants.They are formulated with a unique extreme pressure additive using an inorganic borate compound. ISO 68, 150, 220..