Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Four Ball Extreme Pressure, Weld Load | 50.0 kg | 110 lb (mass) | Mean Hertz Load; IP 239 |
Solvay Specialty Polymers FOMBLIN® LC08 PFPE Lubricant FOMBLIN LC perfluoropolyether fluids have the following unique features: excellent wear characteristics; very good low temperature properties; cost-effective; and outstanding for applications requir.. |
|||
Four Ball Extreme Pressure, Weld Load | 50.0 kg | 110 lb (mass) | Load Weld Index |
ChevronTexaco ISO 460 Ultra Gear Lubricant FeaturesChevron Ultra Gear Lubricants are premium grade, multipurpose gear lubricants.They are formulated with a unique extreme pressure additive using an inorganic borate compound. ISO 68, 150, 220.. |