Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Four Ball Extreme Pressure, Weld Load | 100 kg | 221 lb (mass) | Mean Hertz Load; IP 239 |
Solvay Specialty Polymers FOMBLIN® LC55 PFPE Lubricant FOMBLIN LC perfluoropolyether fluids have the following unique features: excellent wear characteristics; very good low temperature properties; cost-effective; and outstanding for applications requir.. |
|||
Four Ball Extreme Pressure, Weld Load | 100 kg | 221 lb (mass) | Mean Hertz Load; IP 239 |
Solvay Specialty Polymers FOMBLIN® LC80 PFPE Lubricant FOMBLIN LC perfluoropolyether fluids have the following unique features: excellent wear characteristics; very good low temperature properties; cost-effective; and outstanding for applications requir.. |