Polymer Property : Four Ball Extreme Pressure, Weld Load = 221 lb (mass) Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 100 kg
221 lb (mass)
Mean Hertz Load; IP 239
Solvay Specialty Polymers FOMBLIN® LC55 PFPE Lubricant
FOMBLIN LC perfluoropolyether fluids have the following unique features: excellent wear characteristics; very good low temperature properties; cost-effective; and outstanding for applications requir..
Four Ball Extreme Pressure, Weld Load 100 kg
221 lb (mass)
Mean Hertz Load; IP 239
Solvay Specialty Polymers FOMBLIN® LC80 PFPE Lubricant
FOMBLIN LC perfluoropolyether fluids have the following unique features: excellent wear characteristics; very good low temperature properties; cost-effective; and outstanding for applications requir..