Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 85.0 kJ/m² | 40.4 ft-lb/in² | ASTM D256 |
Solvay TECHNYL® A 218 V25 NAT BA PA66, 25% glass fiber, DRY Description: Polyamide 66, reinforced with 25% of glass fiber, specially stabilized to improve its resistance to oils and greases, for injection molding.Available in: Asia PacificProduct Application.. |
|||
Izod Impact, Notched (ISO) | 85.0 kJ/m² | 40.4 ft-lb/in² | ISO 180/1eA |
Solvay TECHNYL® C 442 Black V PA6, DRY Description: Unreinforced polyamide PA6, high viscosity, with high flexibility and very high impact resistance even at low temperature, for extrusion.Available in: Europe Product Applications: It ha.. |
|||
Izod Impact, Notched (ISO) | 85.0 kJ/m² | 40.4 ft-lb/in² | ISO 180 |
Polyram RamTough PZ780 Polycarbonate, UV Stabilized General purpose, UV stabilized polycarbonate for injection molding applications.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 85.0 kJ/m² @Thickness 3.20 mm, Temperature 23.0 °C |
40.4 ft-lb/in² @Thickness 0.126 in, Temperature 73.4 °F |
partial break; b.o. ISO 180-A |
Covestro Makrolon® Rx2635 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices• Med.. |