Material Notes:
General purpose, UV stabilized polycarbonate for injection molding applications.Information provided by Polyram.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cm
0.0050 - 0.0080 in/in
ISO 2577
Melt Flow 10 g/10 min

@Load 1.20 kg,
Temperature 300 °C
10 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 70.0 MPa
10200 psi
ISO 527
Elongation at Break 65 %
65 %
ISO 527
Tensile Modulus 2.40 GPa
348 ksi
ISO 527
Flexural Strength 98.0 MPa
14200 psi
ISO 178
Flexural Modulus 2.35 GPa
341 ksi
ISO 178
Izod Impact, Notched (ISO) 85.0 kJ/m²
40.4 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 137 °C
279 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 124 °C
255 °F
ISO 75
Vicat Softening Point 145 °C
293 °F
ISO 306
Flammability, UL94 V-2

@Thickness 3.00 mm
V-2

@Thickness 0.118 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
IEC 60093
Surface Resistance 1.00e+15 ohm
1.00e+15 ohm
IEC 60093