Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 83.0 kJ/m²

@Temperature 23.0 °C
39.5 ft-lb/in²

@Temperature 73.4 °F
ISO 180/4A
Styron CALIBREâ„¢ 201-15 Polycarbonate Resin
Overview: CALIBREâ„¢ 201-15 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistanc..
Izod Impact, Notched (ISO) 83.0 kJ/m²

@Temperature 23.0 °C
39.5 ft-lb/in²

@Temperature 73.4 °F
ISO 180/A
Styron CALIBREâ„¢ 301-15 Polycarbonate Resin
Overview: CALIBREâ„¢ 300-115 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity. The CALIBREâ„¢ 300-10 series products are available in 4 ..
Izod Impact, Notched (ISO) 83.0 kJ/m²

@Temperature 23.0 °C
39.5 ft-lb/in²

@Temperature 73.4 °F
ISO 180/A
Styron CALIBREâ„¢ 701-15 Polycarbonate Resin
Overview: CALIBREâ„¢ 701-15 Series resins are formulated and produced to supply both clarity and enhanced ignition resistance. They do so while maintaining excellent physical properties and proce..
Izod Impact, Notched (ISO) 83.0 kJ/m²

@Temperature 23.0 °C
39.5 ft-lb/in²

@Temperature 73.4 °F
ISO 180/A
Styron CALIBREâ„¢ 703-15 Polycarbonate Resin
Overview: CALIBREâ„¢ 701-15 Series resins are formulated and produced to supply both clarity and enhanced ignition resistance. They do so while maintaining excellent physical properties and proce..
Izod Impact, Notched (ISO) 83.0 kJ/m²

@Temperature 23.0 °C
39.5 ft-lb/in²

@Temperature 73.4 °F
ISO 180/A
Styron CALIBREâ„¢ 303-15 Polycarbonate Resin
Overview: CALIBREâ„¢ 300-115 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity. The CALIBREâ„¢ 300-10 series products are available in 4 ..