Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 16.6 kJ/m²

@Temperature -40.0 °C
7.90 ft-lb/in²

@Temperature -40.0 °F
ISO Test
BASF Ultramid® TG7S BK-102 35% Glass Filled PA6 (Dry)
Ultramid TG7S is a 34% glass reinforced, heat stabilized, impact modified nylon 6 injection molding grade. It was developed to meet the demanding requirements of the first North American seat cushi..
Izod Impact, Notched (ISO) 16.6 kJ/m²
7.90 ft-lb/in²
ISO 180-1A
Gromax CFG33-QS11N1 Nylon 6 33% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.