Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 16.6 kJ/m² @Temperature -40.0 °C |
7.90 ft-lb/in² @Temperature -40.0 °F |
ISO Test |
BASF Ultramid® TG7S BK-102 35% Glass Filled PA6 (Dry) Ultramid TG7S is a 34% glass reinforced, heat stabilized, impact modified nylon 6 injection molding grade. It was developed to meet the demanding requirements of the first North American seat cushi.. |
|||
Izod Impact, Notched (ISO) | 16.6 kJ/m² | 7.90 ft-lb/in² | ISO 180-1A |
Gromax CFG33-QS11N1 Nylon 6 33% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |