Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 62.0 kJ/m² | 29.5 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP DI001L PC LNP* LUBRICOMP* DI001L is a compound based on Polycarbonate resin containing 2% Silicone. Added characteristics of this grade are: Low Extractable. |
|||
Izod Impact, Notched (ISO) | 62.0 kJ/m² @Temperature -30.0 °C |
29.5 ft-lb/in² @Temperature -22.0 °F |
|
Polimeri Europa KOBLEND HI 18 PBT+PC, Impact Grade
(discontinued **) Symbol according to ISO 1043/1: PBT+PC-HI Elastomer modified PBT+PC blend, similar to KOBLEND HI 10 with improved impact resistance at low temperatures and better thermal properties. Main applicat.. |
|||
Izod Impact, Notched (ISO) | 62.0 kJ/m² | 29.5 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® X5601WX PBT + PC + PET Impact modified PBT+PC+PET, Heat aging improved Xenoy |
|||
Izod Impact, Notched (ISO) | 62.0 kJ/m² | 29.5 ft-lb/in² | ISO 180, Ductile break |
DSM Fibre Intermediates Nyrim® 3000 (Dry) Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is processed via Reaction Injection Moulding (RIM) tec.. |