Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 60.0 kJ/m² @Temperature 0.000 °C |
28.6 ft-lb/in² @Temperature 32.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® 1173X PC Copolymer (Europe-Africa-Middle East) Lexan* 1173X polycarbonate (PC) resin is a high flow, UV stabilized injection molding grade. This resin offers good low temperature (-30 C) ductility in combination with high flow characteristics an.. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1414 PC Copolymer (Asia Pacific) Lexan* EXL1414 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductility in combination with excel.. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1444 PC Copolymer Lexan* EXL1444 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade suitable for FDA compliant applications. This resin offers extreme low temperature (-.. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1444 PC Copolymer (Asia Pacific) Lexan* EXL1444 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade suitable for FDA compliant applications. This resin offers extreme low temperature (-.. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1890T PC Copolymer Lexan* EXL1890T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade for food contact applications. This resin offers cold temperature (0 °C) ductility in combin.. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1890T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1890T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade for food contact applications. This resin offers cold temperature (0 °C) ductility in combin.. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXE1414 PC Copolymer Lexan* FXE1414 polycarbonate (PC) siloxane copolymer resin is a special effects fluorescent, medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductil.. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HF1110 PC (Europe-Africa-Middle East) LEXAN HF1110 is a high flow grade especially designed for applications that require thin wall sections and high flow lengths. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HF1130R PC (Europe-Africa-Middle East) LEXAN HF1130R is a high flow, UV stabilized, grade especially designed for applications that require thin wall sections and higher flow lengths. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HF1140R PC (Europe-Africa-Middle East) LEXAN HF1140R is a high flow grade. This material is especially designed for applications that require thin wall sections and high flow lengths. FDA food contact compliant in limited colors.Effect.. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HP1NREU PC (Europe-Africa-Middle East) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains no mold release. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HP1REU PC (Europe-Africa-Middle East) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains mold release. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HP2 PC (Europe-Africa-Middle East) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains m.. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HPS2 PC (Europe-Africa-Middle East) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam and gamma sterilizable.. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HPS2S PC (Europe-Africa-Middle East) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma steriliza.. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HPX8R PC Copolymer (Asia Pacific) Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o.. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® ML6413 PC Lexan* ML6413 resin is an impact modified, flame retardant polycarbonate grade with Br- & Cl-free FR systems. It features improved light shielding capability with good flow, impact and thermal prope.. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXR123R PC (Europe-Africa-Middle East) Lexan FXR123R Resin |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HF1140 PC (Europe-Africa-Middle East) Ideal for disposables/short life cycles. Good clarity, heat resistance, property retention and dimensional stability. FDA food contact compliant in limited colors.Effective January 15th, 2007 this.. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HP2NR PC Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no.. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP DX11354X PC (Asia Pacific) LNP* Thermocomp* Compound DX11354X is a colorable PC based compound with stable plating and RF performance, colored LDS material solution, good surface and processing window, high impact strength. I.. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | ISO 180/A |
Tisan TISSAN® UNR Styrene Acrylonitrile Properties:Natural or ColoredGlass fiber and glass beadMineral filledFlame retardantGood thermal and chemical resistanceExcellent transparencyExcellent mechanical propertiesDimensional stabilityEasy.. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | ISO 180-93 |
Wellman Wellamid® XT1668-BK1 High Impact Nylon 66 Description: High Impact Nylon 66Information provided by Wellman. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | ISO 180 |
Polyram RamTough PZ126 Polycarbonate, Low Viscosity General purpose, low viscosity polycarbonate for injection molding applications.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² @Thickness >=5.00 mm |
28.6 ft-lb/in² @Thickness >=0.197 in |
24hr/23°C/50% RH; ISO 180/2A; IEC/EN 60893-2 5.4.3 |
Elektro-Isola G-Etronax EP 215 S Epoxy, Glass Fabric Reinforcement, Green, Sheets Description: Particularly good, lasting strength properties and insulation values even at high application temperatures. Radiation-resistant. Can be used at cryogenic temperatures. Very good where t.. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² @Thickness >=5.00 mm |
28.6 ft-lb/in² @Thickness >=0.197 in |
24hr/23°C/50% RH; ISO 180/2A; IEC/EN 60893-2 5.4.3 |
Elektro-Isola G-Etronax PM H Polyester, Glass Mat, Creme, Sheets Description: A reasonably-priced alternative to other high-temperature types. Low thermal conductivity. Applications: Used as, among other things, thermal insulation plates where high strength prope.. |
|||
Izod Impact, Notched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | ISO 180 |
Polyram RamLloy PVB702 Nylon/ABS Alloy, Impact Modified Impact modified, UV stabilized Nylon/ABS alloy for injection molding applications.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 60.0 - 80.0 kJ/m² | 28.6 - 38.1 ft-lb/in² | Average value: 66.7 kJ/m² Grade Count:6 |