Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 5.00 - 6.00 kJ/m²

@Temperature -40.0 - -30.0 °C
2.38 - 2.86 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 5.67 kJ/m² Grade Count:3
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are..
Izod Impact, Notched (ISO) 6.00 - 6.00 kJ/m²

@Temperature -30.0 - -30.0 °C
2.86 - 2.86 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 6.00 kJ/m² Grade Count:1
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar..
Izod Impact, Notched (ISO) 4.00 - 6.00 kJ/m²
1.90 - 2.86 ft-lb/in²
Average value: 4.83 kJ/m² Grade Count:6
Overview of materials for Acetal Homopolymer, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Glass Fiber Reinforced". Each property range of values reported is minimum and maxim..
Izod Impact, Notched (ISO) 5.00 - 6.00 kJ/m²

@Temperature -30.0 - -30.0 °C
2.38 - 2.86 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 5.67 kJ/m² Grade Count:3
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe..
Izod Impact, Notched (ISO) 4.60 - 6.00 kJ/m²
2.19 - 2.86 ft-lb/in²
Average value: 5.53 kJ/m² Grade Count:3
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled". Specific grades with glass content betwe..
Izod Impact, Notched (ISO) 5.10 - 6.00 kJ/m²
2.43 - 2.86 ft-lb/in²
Average value: 5.40 kJ/m² Grade Count:4
Overview of materials for Polyetherimide (PEI), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu..
Izod Impact, Notched (ISO) 3.00 - 6.00 kJ/m²

@Temperature -40.0 - -20.0 °C
1.43 - 2.86 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 4.00 kJ/m² Grade Count:5
Overview of materials for Nylon 66, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum ..
Izod Impact, Notched (ISO) 3.00 - 6.00 kJ/m²

@Temperature -40.0 - -20.0 °C
1.43 - 2.86 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 4.50 kJ/m² Grade Count:2
Overview of materials for Nylon 66, 20% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Carbon Fiber Filled". Specific grades with carbon fiber content between 15% and 24% are in..
Izod Impact, Notched (ISO) 3.00 - 6.00 kJ/m²

@Temperature -30.0 - -30.0 °C
1.43 - 2.86 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 4.67 kJ/m² Grade Count:3
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced". Each property range of values repo..
Izod Impact, Notched (ISO) 2.70 - 6.00 kJ/m²
1.28 - 2.86 ft-lb/in²
Average value: 4.53 kJ/m² Grade Count:12
Overview of materials for Acetal Copolymer, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu..
Izod Impact, Notched (ISO) 6.00 - 6.00 kJ/m²

@Temperature -30.0 - -30.0 °C
2.86 - 2.86 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 6.00 kJ/m² Grade Count:1
Overview of materials for Acetal Copolymer, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of ..
Izod Impact, Notched (ISO) 5.00 - 6.00 kJ/m²
2.38 - 2.86 ft-lb/in²
Average value: 5.75 kJ/m² Grade Count:4
Overview of materials for Polycarbonate/ABS Alloy, Antistat/Conductive
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Antistat/Conductive". Each property range of values reported is minimum and max..
Izod Impact, Notched (ISO) 2.70 - 6.00 kJ/m²
1.28 - 2.86 ft-lb/in²
Average value: 3.67 kJ/m² Grade Count:4
Overview of materials for Polypropylene Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Glass Bead Filled". Each property range of values reported is minimum and maximum values o..
Izod Impact, Notched (ISO) 6.00 - 6.00 kJ/m²

@Temperature -30.0 - -30.0 °C
2.86 - 2.86 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 6.00 kJ/m² Grade Count:1
Overview of materials for Polybutylene Terephthalate (PBT), PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), PTFE Filled". Each property range of values reported is minimum and ma..
Izod Impact, Notched (ISO) 6.00 - 6.00 kJ/m²

@Temperature -30.0 - -30.0 °C
2.86 - 2.86 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 6.00 kJ/m² Grade Count:1
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Fiber Filled". Each property range of values reported is minimu..