Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 2.70 - 40.0 kJ/m²
1.28 - 19.0 ft-lb/in²
Average value: 13.1 kJ/m² Grade Count:5
Overview of materials for Polypropylene with 30% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are..
Izod Impact, Notched (ISO) >= 2.70 kJ/m²
>= 1.28 ft-lb/in²
ISO 180-1A
Schwartz Technical Plastics LAMIGAMID® 314 Cast Polyamide 6, MoS2 Filled, Heat Stabilized, Dry
Application: sheaves, wheels, gear-rods, gears, sliding linersInformation provided by Schwartz Technical Plastics GmbH
Izod Impact, Notched (ISO) 2.70 kJ/m²
1.28 ft-lb/in²
ISO 180-1A
Schwartz Technical Plastics LAMIGAMID® 317 Cast Polyamide 6, Heat Stabilized, Dry
Application: coupling parts, sealing rings, bearingsInformation provided by Schwartz Technical Plastics GmbH
Izod Impact, Notched (ISO) 2.70 kJ/m²
1.28 ft-lb/in²
Type 1, Notch A; ISO 180
Solvay Specialty Polymers Amodel® A-8422 LS WH159 Polyphthalamide (PPA), 22% Mineral
Amodel® A-8422 LS is a light-stabilized, high-reflectivity, 22%-reinforced white polyphthalamide (PPA) that exhibits high heat resistance, high strength and stiffness over a broad temperature ran..
Izod Impact, Notched (ISO) 2.70 - 6.00 kJ/m²
1.28 - 2.86 ft-lb/in²
Average value: 4.53 kJ/m² Grade Count:12
Overview of materials for Acetal Copolymer, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu..
Izod Impact, Notched (ISO) 2.70 - 6.00 kJ/m²
1.28 - 2.86 ft-lb/in²
Average value: 3.67 kJ/m² Grade Count:4
Overview of materials for Polypropylene Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Glass Bead Filled". Each property range of values reported is minimum and maximum values o..
Izod Impact, Notched (ISO) 2.70 - 54.0 kJ/m²
1.28 - 25.7 ft-lb/in²
Average value: 19.0 kJ/m² Grade Count:11
Overview of materials for Polypropylene with 10% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Talc Filler". Specific grades with primary filler content between 5% and 14% are ..
Izod Impact, Notched (ISO) 2.70 kJ/m²
1.28 ft-lb/in²
ISO 180
Polyram RamTal PM340S6 Polyacetal for Injection Molding, 30% Glass-Beads Filled
30% Glass-beads filled polyacetal for injection molding applications.Information provided by Polyram.