Polymer Property : Izod Impact, Notched (ISO) = 5.57 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 11.7 kJ/m²
5.57 ft-lb/in²
ISO 180/1A
Celanese Celanex® 4202 PBT, 15% Glass Reinforced  (Unverified Data**)
Celanex 4202 is a 15% glass reinforced, impact modified polybutylene terephthalate with excellent surface appearance.15% glass-fiber, improved impactInformation provided by Celanese
Izod Impact, Notched (ISO) 11.7 kJ/m²
5.57 ft-lb/in²
ISO 180/1A
Celanese CELANEX 3300HR PBT, 30% Glass Reinforced
Celanex 3300HR is a 30% glass reinforced polybutylene terephthalate which has excellent hydrolysis resistance, mechanical properties and processabilityInformation provided by Celanese
Izod Impact, Notched (ISO) 11.7 kJ/m²
5.57 ft-lb/in²
ISO 180/1A
Celanese CELANEX 4202 PBT, 15% Glass Reinforced
Celanex 4202 is a 15% glass reinforced, impact modified polybutylene terephthalate with excellent surface appearance.Information provided by Celanese
Izod Impact, Notched (ISO) 11.7 kJ/m²
5.57 ft-lb/in²
ISO 180/1A
Celanese Celanex® 3300HR PBT, 30% Glass Reinforced
Celanex 3300HR is a 30% glass reinforced polybutylene terephthalate which has excellent hydrolysis resistance, mechanical properties and processabilityTo avoid hydrolytic degradation during processi..
Izod Impact, Notched (ISO) 11.7 kJ/m²
5.57 ft-lb/in²
ISO 180/1A
Celanese Celanex® 6406 PBT, 40% Mineral / Glass Reinforced
Celanex 6406 is a 40% mineral/glass reinforced resin providing excellent toughness combined with warpage resistance, surface gloss and good mechanical properties. Celanex 6406 is particularly suited..
Izod Impact, Notched (ISO) 11.7 kJ/m²
5.57 ft-lb/in²
ISO Test
BASF Ultraform N 2640 Z4 BK140 Q600 POM
Ultraform N2640 Z4 BK140 Q600 is a high toughness, elastomer-modified injection molding POM grade.