Polymer Property : Izod Impact, Notched (ISO) = 5.39 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 5.39 kJ/m²
2.56 ft-lb/in²
Type A; ISO 180:2000
Nylacast Moly Cast Nylon 6, MoS2 Filled
Nylacast Moly is part of the Cast Nylon 6 family. Its improved crystallization occurs by the addition of Molybdenum Disulphide. It includes MoS2, which is an extremely effective self dry lubricant w..