Polymer Property : Izod Impact, Notched (ISO) = 4.90 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 10.3 kJ/m²
4.90 ft-lb/in²
ISO 180-1A
Gromax BFG30-BN00B2 Nylon 6 33% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
Izod Impact, Notched (ISO) 10.3 kJ/m²
4.90 ft-lb/in²
GB/T 1843-2008
Sichuan Deyang Haton® hGR60 Polyphenylene Sulfide, Glass Fiber Reinforced
Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD