Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 4.10 kJ/m² | 1.95 ft-lb/in² | ISO 180/1A |
Fiberfil® J-60/20/TT/FD WT8381 Polypropylene Homopolymer, 20% Glass Reinforced, FDA compliant Information provided by FIBERFIL Engineered Plastics |
|||
Izod Impact, Notched (ISO) | 4.10 kJ/m² | 1.95 ft-lb/in² | ISO 180-1A |
Gromax BFG15-DN00N1 Nylon 6 16% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |