Fiberfil® J-60/20/TT/FD WT8381 Polypropylene Homopolymer, 20% Glass Reinforced, FDA compliant

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer FiberFil
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fiberfil® J-60/20/TT/FD WT8381 Polypropylene Homopolymer, 20% Glass Reinforced, FDA compliant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by FIBERFIL Engineered Plastics
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
Melt Flow 19 g/10 min
19 g/10 min
230/2.16 (typical); ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 48.0 MPa
6960 psi
ISO 527
Elongation at Yield 2.5 %
2.5 %
ISO 527
Flexural Strength 73.50 MPa
10660 psi
ISO 178
Flexural Modulus 2.90 GPa
420 ksi
ISO 178
Izod Impact, Notched (ISO) 4.10 kJ/m²
1.95 ft-lb/in²
ISO 180/1A
Izod Impact, Unnotched (ISO) 19.5 kJ/m²
9.28 ft-lb/in²
ISO 180/1U