Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched (ISO) = 37.0 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 37.0 kJ/m²
17.6 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics NORYL WCV063 PPE+SEBS+Polyolefin
Flexible, non-halogenated FR, mPPE extrusion grade material for evaluation in automotive wire coating applications requiring ISO6722.
Izod Impact, Notched (ISO) 37.0 kJ/m²
17.6 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics NORYL WCV063 PPE+SEBS+Polyolefin (Asia Pacific)
Flexible, non-halogenated FR, mPPE extrusion grade material for evaluation in automotive wire coating applications requiring ISO6722.
Izod Impact, Notched (ISO) 37.0 kJ/m²
17.6 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics NORYL WCV063 PPE+SEBS+Polyolefin (Europe-Africa-Middle East)
Flexible, non-halogenated FR, mPPE extrusion grade material for evaluation in automotive wire coating applications requiring ISO6722.
Izod Impact, Notched (ISO) 37.0 kJ/m²
17.6 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP LUBRICOMP PDXF89080 PE
LNP* LUBRICOMP* PDXF89080 is a compound based on Polyethylene containing Proprietary Fillers. Added feature of this grade is: Wear Resistant.
Izod Impact, Notched (ISO) 37.0 kJ/m²

@Temperature 23.0 °C
17.6 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP Stat-kon TE002
LNP* Stat-kon* TE002 is a compound based on Polyurethane resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the A..
Izod Impact, Notched (ISO) 37.0 kJ/m²
17.6 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP STAT-KON TE002 PU
LNP* STAT-KON* TE002 is a compound based on Polyurethane resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive.
Izod Impact, Notched (ISO) 37.0 kJ/m²
17.6 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP THERMOCOMP 2Z004 ETFE
LNP* THERMOCOMP* 2Z004 is a compound based on ETFE resin containing 20% Milled Glass.
Izod Impact, Notched (ISO) 37.0 kJ/m²

@Temperature 23.0 °C
17.6 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP Thermocomp 2Z004 FP-E (EFTE)
LNP* 2Z004 is a compound based on Ethylenetetrafluoroethylene (ETFE) containing Milled Glass.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched (ISO) 37.0 kJ/m²

@Temperature 23.0 °C
17.6 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP Thermocomp YF004 Polyester Elastomer
LNP THERMOCOMP* YF004 is a compound based on Polyester Elastomer resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched (ISO) 37.0 kJ/m²
17.6 ft-lb/in²
ISO 180/1eA
Lubrizol ESTALOC® T5160 Ether-Type, Reinforced Engineering Thermoplastic (European Grade)
Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio..
Izod Impact, Notched (ISO) 37.0 kJ/m²
17.6 ft-lb/in²
80x10x4; ISO 180/1A
Eurostar Starpylen HT 25 MC PP, Mineral Filled, Injection Molding
Starpylen HT 25 MC is a Mineral Filled Polypropylene Injection Molding ResinInformation provided by Eurostar.
Izod Impact, Notched (ISO) 37.0 kJ/m²
17.6 ft-lb/in²
ISO 180/1A
Total Lacqrene® 9218 Polystyrene  (discontinued **)
LACQRENE® 9218 is a polystyrene modified with polyethylene. This combination gives a high level of stress crack resistance with excellent mechanical properties and good abrasion resistance. This ..
Izod Impact, Notched (ISO) 37.0 kJ/m²

@Temperature -30.0 °C
17.6 ft-lb/in²

@Temperature -22.0 °F
Polimeri Europa KOBLEND PCA 839 PC+ABS  (discontinued **)
Symbol according to ISO 1043/1: PC+ABS Injection moulding grade with very good impact behaviour even at low temperatures, good dimensional stability. Vicat/B50 = 130°C Main applications fields: a..
Izod Impact, Notched (ISO) 37.0 kJ/m²
17.6 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP VERTON RV00CEXS PA 66
LNP* VERTON* RV00CEXS is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this grade include: Easy Molding, Structural.