Polymer Property : Izod Impact, Notched (ISO) = 33.3 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 8.00 - 70.0 kJ/m²
3.81 - 33.3 ft-lb/in²
Average value: 28.6 kJ/m² Grade Count:14
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m..
Izod Impact, Notched (ISO) 4.50 - 70.0 kJ/m²
2.14 - 33.3 ft-lb/in²
Average value: 13.0 kJ/m² Grade Count:88
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25..
Izod Impact, Notched (ISO) 13.0 - 70.0 kJ/m²
6.19 - 33.3 ft-lb/in²
Average value: 39.8 kJ/m² Grade Count:5
Overview of materials for Polycarbonate, Gamma Radiation Resistant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Gamma Radiation Resistant". Each property range of values reported is minimum and maximum..