Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 3.10 - 31.0 kJ/m² | 1.48 - 14.8 ft-lb/in² | Average value: 8.98 kJ/m² Grade Count:19 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min.. |
|||
Izod Impact, Notched (ISO) | 7.00 - 31.0 kJ/m² | 3.33 - 14.8 ft-lb/in² | Average value: 13.7 kJ/m² Grade Count:13 |
Overview of materials for Acetal Copolymer, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values.. |