Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 8.00 - 44.0 kJ/m²
3.81 - 20.9 ft-lb/in²
Average value: 14.6 kJ/m² Grade Count:32
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a..