Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 2.75 - 2.95 kJ/m²
1.31 - 1.40 ft-lb/in²
ISO 180
Tisan TISMOSET®
Properties:Flame retardantHigh gloss surfaceImproved thermal and electircal strengthHigh impact strengthMinimized shrinkage at the presence of moldingHigh melting flow indexReduced moisture absorpti..