Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 27.0 - 176 kJ/m²
12.8 - 83.7 ft-lb/in²
Average value: 75.7 kJ/m² Grade Count:8
Overview of materials for High Density Polyethylene (HDPE), Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Impact Grade". Each property range of values reported is minimum and m..