Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 33.5 - 33.5 kJ/m² @Temperature -30.0 - -30.0 °C |
15.9 - 15.9 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 33.5 kJ/m² Grade Count:1 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced". Each property range of values reported is mi.. |