Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 7.50 - 10.5 kJ/m² @Temperature -20.0 - -20.0 °C |
3.57 - 5.00 ft-lb/in² @Temperature -4.00 - -4.00 °F |
Average value: 8.82 kJ/m² Grade Count:4 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyether Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyether Grade". Each property range of values reported is minimum a.. |