Mechanical Properties Metric English Comments
Modulus of Rigidity 0.2138 GPa

@Temperature -40.0 °C
31.01 ksi

@Temperature -40.0 °F
ASTM D1053
Lubrizol ESTANE® 58212 Ether Based Thermoplastic Polyurethane
Features: Excellent clarity and UV stable with good melt strength. Pre-drying: 2 hours at 104°C (220°F) in dehumidifying hopper dryerUses: Extrusion: Cable jacket, hose/tube, profile and film and ..