Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Multi-axial Impact @ -30°C Total Energy | 15.0 J @Thickness 3.00 mm, Temperature 23.0 °C |
11.1 ft-lb @Thickness 0.118 in, Temperature 73.4 °F |
Injection Molded, Ductile Failure; ISO 6603-2 |
Styron DLGF9411.00 Polypropylene Overview: DLGF 9400.00 is a 40% long glass fiber reinforced grade with good flow properties. The glass fibers (12 mm length) are coupled to the polypropylene matrix resulting in high stiffness and s.. |