Polymer Property : Izod Impact, Unnotched (ISO) = 96.0 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 90.0 - 96.0 kJ/m²

@Temperature -30.0 - -30.0 °C
42.8 - 45.7 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 92.0 kJ/m² Grade Count:3
Overview of materials for Nylon 66, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. ..