Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 180 kJ/m²
85.7 ft-lb/in²
80*10*3; ISO 180/1U
SABIC Innovative Plastics Lexan® LUX2619 PC (Europe-Africa-Middle East)
Lexan* LUX2619 Polycarbonate resin is an extrusion grade. It is UL94 V-2 rated at 1.5 mm. It was designed for high light reflectance.
Izod Impact, Unnotched (ISO) 180 kJ/m²

@Temperature -30.0 °C
85.7 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1U
SABIC Innovative Plastics Lexan® ML7682 PC Copolymer (Asia Pacific)
Lexan ML7682 resin is a flame retardant polycarbonate blend featuring high flow, good processability, good impact, good heat resistance, and UV stability. It is of non-chlorine and non-bromine flame..
Izod Impact, Unnotched (ISO) 180 kJ/m²
85.7 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP DX98306H PC
LNP* LUBRICOMP* DX98306H is a compound based on Polycarbonate resin containing Proprietary Fillers. Added features of this material include: Wear Resistant, Low Extractible.
Izod Impact, Unnotched (ISO) 180 kJ/m²
85.7 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP DX98306H PC (Asia Pacific)
LNP* Lubricomp* DX98306H is a compound based on Polycarbonate resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated, Low Extractible.
Izod Impact, Unnotched (ISO) 180 kJ/m²
85.7 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP STAT-LOY 9X07438 ASA+PC
LNP* STAT-LOY* 9X07438 is a compound based on Polycarbonate/ASA containing Proprietary Filler(s). Added features of this grade include: Antistatic, Colorable, Weatherable.