Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 179 kJ/m²
85.2 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP DI001L PC
LNP* LUBRICOMP* DI001L is a compound based on Polycarbonate resin containing 2% Silicone. Added characteristics of this grade are: Low Extractable.
Izod Impact, Unnotched (ISO) 179 kJ/m²
85.2 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP DX07404H PC
LNP* LUBRICOMP* DX07404H is a compound based on Polycarbonate containing Proprietary Fillers. Added features of this grade are: Healthcare, Wear Resistant.