Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 70.2 kJ/m² | 33.4 ft-lb/in² | ISO 180 |
LNP Thermocomp® STN-F-1006 HS Polyamide 46, Glass Fiber Reinforcement
(discontinued **) Features: Heat StabilizedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are sti.. |