Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 15.0 - 15.0 kJ/m²

@Temperature -30.0 - -30.0 °C
7.14 - 7.14 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 15.0 kJ/m² Grade Count:1
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe..