Polymer Property : Izod Impact, Unnotched (ISO) = 64.0 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 64.0 kJ/m²
30.5 ft-lb/in²
80*10*3; ISO 180/1U
SABIC Innovative Plastics Lexan® HFD4211 PC
Lexan* HFD4211 is a 10% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release.
Izod Impact, Unnotched (ISO) 64.0 kJ/m²
30.5 ft-lb/in²
80*10*3; ISO 180/1U
SABIC Innovative Plastics Lexan® HFD4211 PC (Asia Pacific)
Lexan* HFD4211 is a 10% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release.
Izod Impact, Unnotched (ISO) 64.0 kJ/m²
30.5 ft-lb/in²
ISO 180
Solvay Specialty Polymers AvaSpire® AV-651 GF30 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-651 GF30 is a 30% glass fiber reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide higher mechanical strength and stiffness than unfilled AV-651 resin. ..
Izod Impact, Unnotched (ISO) 64.0 kJ/m²
30.5 ft-lb/in²
80*10*3; ISO 180/1U
SABIC Innovative Plastics Lexan® HFD4211 PC (Europe-Africa-Middle East)
Lexan* HFD4211 is a 10% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release.
Izod Impact, Unnotched (ISO) 64.0 kJ/m²
30.5 ft-lb/in²
ISO 180
Solvay Specialty Polymers AvaSpire® AV-651 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber
AvaSpire® AV-651 GF30 is a 30% glass fiber reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide higher mechanical strength and stiffness than unfilled AV-651 res..
Izod Impact, Unnotched (ISO) 64.0 kJ/m²
30.5 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP RC006XXH PA 66
LNP* THERMOCOMP* RC006XXH is a compound based on Nylon 66 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Healthcare.
Izod Impact, Unnotched (ISO) 64.0 kJ/m²
30.5 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP YF002 POLYESTER ELASTOMER
LNP* THERMOCOMP* YF002 is a compound based on Poyester Elastomer containing 10% Glass Fiber. Added feature of this grade is: High Modulus.
Izod Impact, Unnotched (ISO) 64.0 kJ/m²
30.5 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOTUF WF006I PBT
LNP THERMOTUF* WF006I is a compound based on PBT containing 30% Glass Fiber. Added features of this material include: High Impact.
Izod Impact, Unnotched (ISO) 64.0 kJ/m²
30.5 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP RX98372H PA 66
LNP* Thermocomp* RX98372H is a compound based on Nylon 66 resin containing Proprietary Fillers. Characteristics of this grade are: Healthcare.
Izod Impact, Unnotched (ISO) 64.0 kJ/m²

@Temperature 23.0 °C
30.5 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Thermotuf WF006I Polyester, TP
LNP THERMOTUF* WF006I is a compound based on Polyester, TP resin containing Glass Fiber. Added features of this material include: High Impact.This data was supplied by SABIC-IP for the Americas reg..
Izod Impact, Unnotched (ISO) 64.0 kJ/m²
30.5 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP VERTON PX06418 PA 6
LNP* VERTON* PX06418 is a compound based on Nylon 6 containing proprietary fillers. Added features of this grade are: Heat Stabilized, Structural.