Izod Impact, Unnotched (ISO) 6.50 kJ/m²
3.09 ft-lb/in²
ISO 180/A
BASF Ultrason E 1010 PES
Ultrason E 1010 is an unreinforced, low viscosity injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability.
Izod Impact, Unnotched (ISO) 6.50 kJ/m² - NB
3.09 ft-lb/in² - NB
Average value: 38.8 kJ/m² Grade Count:57
Overview of materials for Polyethersulfone (PES)
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M..